Rubber Composite - an overview | ScienceDirect Topics
The only ingredient that is changed in this series was the silica loading. The ingredients are mixed with NR on the two-roll mill and cross-linked in a mold at 155°C under the pressure of 100–120 kg/cm 2 for 20–30 min to produce cross-linked NR sheets of approximately 1 mm in thickness.